The material is compounded, filtered, stabilized, and processed using PCR
sources, achieving tensile strength and modules exceeding 9000 psi and
3000 MPA, respect ...
The material is compounded, filtered, stabilized, and processed using PCR
sources, achieving tensile strength and modules exceeding 9000 psi and
3000 MPA, respectively